Data Teknis: | ||||||
Matras inti multi-aksial | ||||||
Kode | Berat (g/m2) | Lapisan aksial Big/m2) | Lapisan inti (g/m2) | Lapisan chop (g/m2) | Kandungan kelembapan | Kecepatan basah (≤S) |
EWF600/180/150 | 930 | 600 | 180 | 150 | ≤0.2 | ≤60 |
EWF600/180/300 | 1080 | 600 | 180 | 300 | ≤0.2 | ≤60 |
EWF600/180/600 | 1380 | 600 | 180 | 600 | ≤0.2 | ≤60 |
EWF600/250/600 | 1450 | 600 | 250 | 600 | ≤0.2 | ≤60 |
EWF800/250/300 | 1350 | 800 | 250 | 300 | ≤0.2 | ≤60 |
EWF800/250/450 | 1500 | 800 | 250 | 450 | ≤0.2 | ≤60 |
EWF800/250/600 | 1650 | 800 | 250 | 600 | ≤0.2 | ≤60 |
Matras inti yang dirajang | ||||||
Kode | Berat (g/m2) | Lapisan yang dirajang (g/m2) | Lapisan inti (g/m2) | Kandungan kelembapan | Kecepatan basah (≤S) | |
ES300/180/300 | 780 | 300/300 | 180 | ≤0.2 | ≤60 | |
ES450/180/450 | 1080 | 450/450 | 180 | ≤0.2 | ≤60 | |
ES600/180/600 | 1380 | 600/600 | 180 | ≤0.2 | ≤60 | |
ES750/180/750 | 1680 | 750/750 | 180 | ≤0.2 | ≤60 | |
ES300/250/300 | 850 | 300/300 | 250 | ≤0.2 | ≤60 | |
ES450/250/450 | 1150 | 450/450 | 250 | ≤0.2 | ≤60 | |
ES600/250/600 | 1450 | 600/600 | 250 | ≤0.2 | ≤60 | |
ES750/250/750 | 1750 | 750/750 | 250 | ≤0.2 | ≤60 |