Kemiringan Campuran FeCral | Komposisi kimia % | |||||||||
C | P | S | MN | Si | CR | NI | Al | FE | Re | Lainnya |
max(≤) | ||||||||||
1R13Al4 | 0.12 | 0.025 | 0.025 | 0.7 | ≤1.00 | 12.5-15.0 | ---- | 3.5-4.5 | 0.1 | BAL. |
0C15Al5 | 0.12 | 0.025 | 0.025 | 0.7 | ≤1.00 | 14.5-15.5 | ---- | 4.5-5.3 | 0.1 | BAL. |
0C25Al5 | 0.06 | 0.025 | 0.025 | 0.7 | ≤0.60 | 23.0-26.0 | ≤0.60 | 4.5-6.5 | 0.1 | BAL. |
0C23Al5 | 0.06 | 0.025 | 0.025 | 0.7 | ≤0.60 | 20.5-23.5 | ≤0.60 | 4.2-5.3 | 0.1 | BAL. |
0C21Al6 | 0.06 | 0.025 | 0.025 | 0.7 | ≤1.00 | 19.0-22.0 | ≤0.60 | 5.0-7.0 | 0.1 | BAL. |
0C21Al4 | 0.06 | 0.025 | 0.025 | 0.7 | ≤1.00 | 21.0-23.0 | ≤0.60 | 3.0-5.2 | 0.1 | BAL. |
0C21Al6Nb | 0.05 | 0.025 | 0.025 | 0.7 | ≤0.60 | 21.0-23.0 | ≤0.60 | 5.0-7.0 | 0.1 | BAL. |
A1 | 0.05 | 0.025 | 0.025 | 0.7 | ≤0.40 | 26.5-27.8 | ≤0.60 | 6.0-7.0 | 0.1 | BAL. |
Protes/Grade | NCr 80/20 | NCr 70/30 | NCr 60/15 | NCr 35/20 | NCr 30/20 | |
Komposisi kimia Utama(%) | NI | BAL. | BAL. | 55.0-61.0 | 34.0-37.0 | 30.0-34.0 |
CR | 20.0-23.0 | 28.0-31.0 | 15.0-18.0 | 18.0-21.0 | 18.0-21.0 | |
FE | ≤ 1.0 | ≤ 1.0 | BAL. | BAL. | BAL. | |
Suhu Kerja Maks (celcius) | 1200 | 1250 | 1150 | 1100 | 1100 | |
Resistivitas di 20 derajat celcius (μ Ω · m) |
1.09 | 1.18 | 1.12 | 1.04 | 1.04 | |
Kerapatan(g/cm3) | 8.4 | 8.1 | 8.2 | 7.9 | 7.9 | |
Konduktivitas Termal (KJ/m· h· ) |
60.3 | 45.2 | 45.2 | 43.8 | 43.8 | |
Koefisien Ekspansi Termal(α x 10-6/) | 18 | 17 | 17 | 19 | 19 | |
Titik Melting (celcius) | 1400 | 1380 | 1390 | 1390 | 1390 | |
Naskh (penghapusan) (%) | > 20 | > 20 | > 20 | > 20 | > 20 | |
Struktur Mikrografis | austenite | austenite | austenite | austenite | austenite | |
Sifat Magnet | tidak magnetik | tidak magnetik | tidak magnetik | tidak magnetik | tidak magnetik |